含磷有机聚硅氧烷/地聚物防火涂层在RPUF中的应用

Application of phosphorus-containing organic polysiloxane/geopolymer fireproof coating in RPUF

  • 摘要: 为提高地聚物胶凝材料的抗裂性和与有机基体的粘结性,本文以9, 10-二氢-9-氧杂-10-磷杂菲-10-氧化物(DOPO)和乙烯基三乙氧基硅烷(VTES)为主要原料合成了含磷有机聚硅氧烷(PDV)并用于地聚物胶凝材料改性,然后将其涂覆于硬质聚氨酯泡沫(RPUF)表面作为防火涂层。探究了PDV引入量对地聚物胶凝材料表干时间、抗裂性及粘结强度的作用机制,并考察了有机改性地聚物防火涂层厚度对RPUF阻燃性能和燃烧行为的影响。结果表明,PDV的引入可缩短地聚物涂层的表干时间,并有利于改善其抗裂性和与RPUF基体间的粘结强度;有机改性地聚物涂层可赋予RPUF阻燃/防火能力,能够有效抑制、延缓其燃烧热释放及生烟速率,仅涂覆400 μm厚度RPUF的极限氧指数(LOI)≥48%并可通过UL-94 V-0等级;随着涂层厚度的增加,样品的残炭含量逐渐提高,且PDV的引入未对地聚物胶凝材料的热降解行为产生显著影响。

     

    Abstract: In order to improve the crack resistance and adhesion with organic matrix of geopolymer cementitious materials, a novel phosphorus-containing organic polysiloxane (PDV) was synthesized using 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO) and vinyl triethoxysilane (VTES) as raw materials for the modification of geopolymer cementitious materials. The prepared organic-modified geopolymer cementitious materials were then coated on the surface of the rigid polyurethane foam (RPUF) as a fireproof coating. The effects of PDV content on the surface drying time, crack resistance, and adhesive strength of geopolymer cementitious materials were studied. In addition, the influences of thickness of organic-modified geopolymer fireproof coating on the flame retardant performance and combustion behavior of RPUF were investigated. The results show that the introduction of PDV shortens the surface drying time of geopolymer coating, and is beneficial to improve its crack resistance and adhesive strength with RPUF matrix. The organic-modified geopolymer coating can endow RPUF with flame retardancy/fire resistance, and effectively inhibit the heat release rate and smoke production rate during combustion. Specifically, the coated RPUF (400 μm) can achieve UL-94 V-0 certification, and its limit oxygen index (LOI) is greater than 48%. With the increase of coating thickness, the char residue of the prepared samples gradually increases. Importantly, the introduction of PDV has no significant impact on the thermal degradation behavior of geopolymer cementitious materials.

     

/

返回文章
返回