Abstract:
Alkaline solution treatment was used to purify B
4C powder and enhance the wetting ability between the B
4C powder and the Mg-Li matrix. The results show that both of the specific surface and B
2O
3 decrease. Tensile strength and density of the pre-mixed alloy prepared by the B
4C powder after alkaline treatment increase. Fewer agglomerates and uniform formation are proved in the metallographic structure of the B
4C/Mg-Li composite (Mg-15Li-2Al-6B
4C). The tensile strength of B
4C/Mg-Li composite increases 21.53% compared with that prepared by B
4C without alkaline solution treatment. Results indicate that the alkaline solution treatment of B
4C powder can improve the strengthening effect of the boride in-situ reacted in the B
4C/Mg-Li composite.