碱式硫酸镁晶须/橡胶复合材料的制备

Preparation and characterization of magnesium oxysulfate whiskers/natural rubber composites

  • 摘要: 将超声分散后的硅烷偶联剂3-氨丙基三乙氧基硅烷改性碱式硫酸镁晶须(KH550-MgOSW)分散液加入天然胶乳(NR)中,对其进行补强,制得绿色环保高性能的KH550-MgOSW/NR复合材料。系统研究了KH550-MgOSW/NR复合材料的力学性能、阻燃性能及热稳定性能。结果表明,用KH550改性后的MgOSW与橡胶基体具有很好的相容性。KH550-MgOSW/NR复合材料的力学性能、阻燃性能及热稳定性能均比纯胶有所提高。当KH550-MgOSW与NR质量比为4%时,KH550-MgOSW/NR复合材料的各项性能均达到最佳,300%定伸应力、拉伸强度、撕裂强度、断裂伸长率、交联密度比纯胶胶膜分别提高了25.0%、36.8%、37.3%、11.4%、44.2%,垂直燃烧等级由FV-1提高到了FV-0级,比纯胶的起始热降解温度(T0)、最大热降解温度(Tp)和终止热降解温度(Tf)分别提高了6.2℃、5.2℃和4.1℃。

     

    Abstract: The magnesium oxysulfate whiskers (MgOSW) were modified by silane coupling agent 3-triethoxysilylpropylamine(KH550), and the modified whiskers dispersion liquid was prepared by ultrasonic technology. MgOSW/natural rubber (NR) composites were developed by the blending modified whiskers dispersion liquid with the NR latex. The morphology, mechanical properties, flammability properties and thermalstability properties of the KH550-MgOSW/NR composites were investigated. The results show that modified MgOSW have good compatibility with NR latex matrix. The properties of KH550-MgOSW/NR composites are improved by the incorporation of modified MgOSW into NR matrix.When modified whiskers mass ratio to NR is 4%, the performances of KH550-MgOSW/NR composites achieve optimum results. Compared with pure NR, the modulus at 300%, tensile strength, tear strength, elongation at break and crosslink density of KH550-MgOSW/NR composites are increased by 25.0%, 36.8%, 37.3%, 11.4%, 44.2%, respectively. The flame retardant grade of composites increases from FV-1 to FV-0. The initial thermal degradation temperature (T0), maximum thermal degradation temperature (Tp), and termination of thermal degradation temperature (TTf) of KH550-MgOSW/NR composites markedly increase 6.2℃, 5.2℃ and 4.1℃, respectively, compared to NR.

     

/

返回文章
返回