GAO Shizhuang, XUE Shanbin, ZHANG Peng, et al. Effect of high temperature environment on water absorption and microstructure evolution of strain hardening cementitious composites[J]. Acta Materiae Compositae Sinica, 2022, 39(10): 4778-4787. doi: 10.13801/j.cnki.fhclxb.20220104.002
Citation: GAO Shizhuang, XUE Shanbin, ZHANG Peng, et al. Effect of high temperature environment on water absorption and microstructure evolution of strain hardening cementitious composites[J]. Acta Materiae Compositae Sinica, 2022, 39(10): 4778-4787. doi: 10.13801/j.cnki.fhclxb.20220104.002

Effect of high temperature environment on water absorption and microstructure evolution of strain hardening cementitious composites

doi: 10.13801/j.cnki.fhclxb.20220104.002
  • Received Date: 2021-09-08
  • Accepted Date: 2021-12-24
  • Rev Recd Date: 2021-12-15
  • Available Online: 2022-01-04
  • Publish Date: 2022-08-22
  • At high temperature, the microstructure of strain hardening cementitious composites (SHCC) was damaged, which leaded to the deterioration of mechanical properties, impermeability and microstructure. The evolution of mechanical properties and capillary water absorption law of SHCC specimens with different fiber contents exposed to 20℃ (normal temperature), 105℃, 200℃, 400℃, 600℃ and 800℃ were studied, and the degradation mechanism of macroscopic properties of materials was analyzed from the perspective of microstructure by using low-field nuclear magnetic technology. The results show that when the heating temperature increases from 20℃ to 105℃, the dynamic elastic modulus decreases, but the compressive strength and flexural strength increase. When the heating temperature rises to 200℃, the compressive strength and dynamic elastic modulus of SHCC change little, but when the temperature is higher than 400℃, both of them decrease rapidly. When the heating temperature is increased from 105℃ to 200℃, the flexural strength of SHCC specimen decreases significantly, and when the heating temperature is higher than 400℃, the flexural strength further deteriorates. The fiber content has no obvious regular effect on the residual mechanical properties of SHCC specimen after high temperature. In addition, when the heating temperature is lower than 200℃, SHCC has poor capillary water absorption performance and has a certain capillary infiltration resistance. Above 400℃, the high temperature damage can significantly promote the capillary water absorption rate and the water absorption capacity of SHCC specimen. When the temperature is lower than 200℃, the initial capillary water absorption coefficient of SHCC specimen with higher fiber content increases more rapidly, and the capillary water absorption capacity is stronger. The microstructure of SHCC specimen is relatively dense when the heating temperature is lower than 200℃. When the temperature exceeds 400℃, the melting of fibers inside the SHCC specimen and the generation and propagation of cacks lead to significant deterioration of mechanical properties and improvement of capillary water absorption. In the meantime, the volume fraction of cracks in SHCC specimens increases with the increase of fiber content after high temperature.

     

  • loading
  • [1]
    WANG X S, WU B S, WANG Q Y. Online SEM investigation of microcrack characteristics of concretes at various temperatures[J]. Cement and Concrete Research,2005,35(7):1385-1390. doi: 10.1016/j.cemconres.2004.07.015
    [2]
    VODAK F, TRTIK K, KAPICKOVA O, et al. The effect of temperature on strength-porosity relationship for concrete[J]. Construction and Building Materials,2004,18(7):529-534. doi: 10.1016/j.conbuildmat.2004.04.009
    [3]
    CHAN Y N, LUO X, SUN W. Compressive strength and pore structure of high-performance concrete after exposure to high temperature up to 800°C[J]. Cement and Concrete Research,2000,30(2):247-251. doi: 10.1016/S0008-8846(99)00240-9
    [4]
    NOUMOWE A. Mechanical properties and microstructure of high strength concrete containing polypropylene fibers exposed to temperatures up to 200℃[J]. Cement and Concrete Research,2005,35(11):2192-2198. doi: 10.1016/j.cemconres.2005.03.007
    [5]
    高贯鹏. 高温后PVA-SHCC的力学性能与抗渗性能试验研究[D]. 青岛: 青岛理工大学, 2012.

    GAO Guanpeng. Experimental study on the mechanical properties and anti-permeability of PVA-SHCC after high temperature[D]. Qingdao: Qingdao Technological University, 2012(in Chinese).
    [6]
    PENG Z, DAI Y, DING X, et al. Self-healing behaviour of multiple microcracks of strain hardening cementitious composites (SHCC)[J]. Construction and Building Materials,2018,169:705-715. doi: 10.1016/j.conbuildmat.2018.03.032
    [7]
    LIU L X. Fire performance of high strength concrete materials and structural concrete[D]. Florida: Florida Atlantic University, 2009.
    [8]
    YAN L, XING Y M, LI J J. High-temperature mechanical properties and microscopic analysis of hybrid-fiber-reinforced high-performance concrete[J]. Magazine of Concrete Research,2013,65(3-4):139-147. doi: 10.1680/macr.12.00034
    [9]
    YU J, LIN J, ZHANG Z, et al. Mechanical performance of ECC with high-volume fly ash after sub-elevated temperatures[J]. Construction and Building Materials,2015,99:82-89. doi: 10.1016/j.conbuildmat.2015.09.002
    [10]
    林建辉, 余江滔, VICTOR C L. 超高韧度水泥基复合材料经亚高温处理后的性能[J]. 硅酸盐学报, 2015, 43(5):604-609.

    LIN Jianhui, YU Jiangtao, VICTOR C L. Performance of engineered cementitious composites after treated at sub-high temperatures[J]. Journal of the Chinese Ceramic Society,2015,43(5):604-609(in Chinese).
    [11]
    高丹盈, 赵亮平, 杨淑慧. 纤维矿渣微粉混凝土高温中的劈拉性能[J]. 硅酸盐学报, 2012, 40(5):677-684.

    GAO Danying, ZHAO Liangping, YANG Shuhui. Splitting tensile properties of fiber reinforced ground granulated blast furnace slag concrete at high temperatures[J]. Jour-nal of the Chinese Ceramic Society,2012,40(5):677-684(in Chinese).
    [12]
    褚洪岩, 孙伟, 蒋金洋. 高温作用下牺牲混凝土的损伤演化[J]. 硅酸盐学报, 2016, 44(2):211-217.

    CHU Hongyan, SUN Wei, JIANG Jinyang. Damage evolution of sacrificial concrete subjected to elevated temperatures[J]. Journal of the Chinese Ceramic Society,2016,44(2):211-217(in Chinese).
    [13]
    STELZNER L, POWIERZA B, OESCH T, et al. Thermally-induced moisture transport in high-performance concrete studied by X-ray-CT and 1H-NMR[J]. Construction and Building Materials,2019,224:600-609. doi: 10.1016/j.conbuildmat.2019.07.065
    [14]
    NOUMOWE A N, SIDDIQUE R, DEBICKI G. Permeability of high-performance concrete subjected to elevated temperature (600°C)[J]. Construction and Building Materials,2009,23(5):1855-1861. doi: 10.1016/j.conbuildmat.2008.09.023
    [15]
    LIU J C, HAI T K. Mechanism of PVA fibers in mitigating explosive spalling of engineered cementitious composite at elevated temperature[J]. Cement and Concrete Composites,2018,93:235-245. doi: 10.1016/j.cemconcomp.2018.07.015
    [16]
    KALIFA P, GREGOIRE C, CHRISTOPHE G. High-temperature behaviour of HPC with polypropylene fibers: From spalling to microstructure[J]. Cement and Concrete Research,2001,31(10):1487-1499. doi: 10.1016/S0008-8846(01)00596-8
    [17]
    ZHANG D, DASARI A, TAN K H. On the mechanism of prevention of explosive spalling in ultra-high performance concrete with polymer fibers[J]. Cement and Concrete Research,2018,113:169-177. doi: 10.1016/j.cemconres.2018.08.012
    [18]
    ZHAO H T, DING J, HUANG Y Y, et al. Experimental analysis on the relationship between pore structure and capillary water absorption characteristics of cement-based materials[J]. Structural Concrete,2019,20(5):1750-1762. doi: 10.1002/suco.201900184
    [19]
    谢恩慧, 周春圣. 利用低场磁共振弛豫测孔技术预测水泥基材料的水分渗透率[J]. 硅酸盐学报, 2020, 48(11):1808-1816.

    XIE Enhui, ZHOU Chunsheng. Prediction of water permeability for cement-based material from the pore size distribution achieved by low-field nuclear magnetic resonance relaxation technique[J]. Journal of the Chinese Ceramic Society,2020,48(11):1808-1816(in Chinese).
    [20]
    ZHOU C S, REN F Z, ZENG Q, et al. Pore-size resolved water vapor adsorption kinetics of white cement mortars as viewed from proton NMR relaxation[J]. Cement and Concrete Research,2018,105:31-43. doi: 10.1016/j.cemconres.2017.12.002
    [21]
    陶高梁, 陈银, 袁波, 等. 基于NMR技术及分形理论预测SWRC[J]. 岩土工程学报, 2018, 40(8):1466-1472.

    TAO Gaoliang, CHEN Yin, YUAN Bo, et al. Predicting soil-water retention curve based on NMR technology and fractal theory[J]. Chinese Journal of Geotechnical Engi-neering,2018,40(8):1466-1472(in Chinese).
    [22]
    薛维培, 刘晓媛, 姚直书, 等. 不同损伤源对玄武岩纤维增强混凝土孔隙结构变化特征的影响[J]. 复合材料学报, 2020, 37(9):2285-2293.

    XUE Weipei, LIU Xiaoyuan, YAO Zhishu, et al. Effects of different damage sources on pore structure change characteristics of basalt fiber reinforced concrete[J]. Acta Materiae Compositae Sinica,2020,37(9):2285-2293(in Chinese).
    [23]
    中国国家标准化管理委员会. 钢丝网水泥用砂浆力学性能试验方法: GB/T 7897—2008[S]. 北京: 中国标准出版社, 2008.

    Standardization Administration of the People's Republic of China. Test methods of mechanical properties of mortar for ferrocement: GB/T 7897—2008[S]. Beijing: Standards Press of China, 2008(in Chinese).
    [24]
    LI Y, ZHANG Y, YANG E H, et al. Effects of geometry and fraction of polypropylene fibers on permeability of ultra-high performance concrete after heat exposure[J]. Cement and Concrete Research,2019,116:168-178. doi: 10.1016/j.cemconres.2018.11.009
    [25]
    张彬. 水泥基材料的高温特性及其再水化修复的研究[D]. 武汉: 武汉理工大学, 2012.

    ZHANG Bin. Study on the high temperature characteristics and rehydration repair of cement-based materials[D]. Wuhan: Wuhan Technological University, 2012(in Chinese).
    [26]
    LI Y, TAN K H, YANG E H. Influence of aggregate size and inclusion of polypropylene and steel fibers on the hot permeability of ultra-high performance concrete (UHPC) atelevated temperature[J]. Construction and Building Materials,2018,169:629-637. doi: 10.1016/j.conbuildmat.2018.01.105
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Figures(6)  / Tables(3)

    Article Metrics

    Article views (700) PDF downloads(20) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return