碱激发偏高岭土-矿渣地聚物基本力学性能的环境碱度敏感性影响

Effect of environmental alkalinity on basic mechanical properties of alkali-activated metakaolin-slag geopolymer

  • 摘要: 偏高岭土-矿渣地聚物能够实现固废资源化利用,其力学性能及微观结构受到养护碱度的影响较大。本文基于不同养护碱度(pH = 8~14),从力学性能、孔隙溶液pH、反应度以及微细观结构等方面展开分析。结果表明,偏高岭土反应度随养护pH升高持续增加,而力学性能呈现先增加再减小的趋势,在pH = 13时达到最大值,此时28 d抗压强度为67.51 MPa,抗折强度为10.65 MPa,偏高岭土反应度为68.45%,孔隙率为26.90%,凝胶结构致密。当pH小于12时,由于体系碱度不足,抑制了地聚合过程中的缩聚反应,强度严重降低;而pH = 14时,由于过量OH−的存在,加剧试件泛碱,阻碍硅铝前驱体持续水化反应,造成材料后期力学强度增长受限。养护pH通过调控碱迁移和孔隙溶液碱度,进而影响反应进程与微结构演化,最终调控地聚物力学性能。

     

    Abstract: Metakaolin-slag geopolymers can facilitate the resource utilization of solid wastes, while their mechanical properties and microstructure are significantly affected by curing alkalinity. In this study, curing environments with pH values ranging from 8 to 14 were investigated in terms of mechanical properties, pore solution pH, degree of reaction, and micro- and mesostructural characteristics. The results show that the degree of reaction of metakaolin increases continuously with increasing curing pH, whereas the mechanical properties first increase and then decrease, reaching the maximum at pH = 13. Under this condition, the 28 d compressive strength and flexural strength reach 67.51 MPa and 10.65 MPa, respectively; the degree of reaction of metakaolin is 68.45%, the porosity is 26.90%, and the gel structure is dense. When the curing pH is lower than 12, insufficient alkalinity suppresses the polycondensation reaction during geopolymerization, resulting in a significant reduction in strength. In contrast, at pH = 14, excessive OH− aggravates efflorescence and hinders the continuous hydration reaction of aluminosilicate precursors, thereby limiting later-age strength development. Curing pH regulates alkali migration and pore solution alkalinity, thereby affecting the reaction process and microstructural evolution and ultimately governing the mechanical properties of the geopolymer.

     

/

返回文章
返回