基于十二烷基糖苷/细菌纤维素纳米晶载药乳液体系的海藻酸盐复合水凝胶的制备与性能

Fabrication and properties of alginate composite hydrogels incorporating dodecyl glycoside/bacterial cellulose nanocrystal stabilized drug-loaded emulsion systems

  • 摘要: 针对海藻酸盐水凝胶对疏水性药物负载能力不足的固有缺陷,本文通过将十二烷基糖苷(APG)/细菌纤维素纳米晶(BCNs)复合物协同稳定Pickering乳液的载药性能与钙离子的内源交联作用相结合的技术策略将载药Pickering乳液包封于海藻酸盐水凝胶基质中制备的复合水凝胶(Alg-APG/BCNs),实现了对疏水性三氯生(TCA)药物的有效负载与可控释放。通过硫酸水解和过氧化氢氧化细菌纤维素的方法制备了Zeta电位为−33.4 mV,平均粒径为454.1 nm的BCNs。进而,以采用APG与BCNs复合物构建高效乳化体系,以溶解TCA药物的氯仿溶液为油相,采用高速剪切法制备了载药Pickering乳液。最后,将载药Pickering乳液与海藻酸盐溶液充分混合,通过CaCO3/D-(+)葡萄糖酸-δ-内酯(GDL)体系触发内源交联,使载药Pickering乳液均匀包封于海藻酸盐三维网络中,形成结构稳定的复合水凝胶。实验结果表明,所制备的Alg-APG/BCNs复合水凝胶具有较高的孔隙率(91.60±3.7%),其对TCA的包封率高达91.5±3.8%,并呈现出长达160 h的缓慢持续释放行为,并表现出一定的pH响应释药特性。同时,它在50~400 μg/mL浓度范围内对L929细胞展现出良好的细胞相容性,对革兰氏阴性菌大肠杆菌(E. coli)与革兰氏阳性菌金黄色葡萄球菌(S. aureus)表现出显著的抗菌效果,且对脂多糖(LPS)诱导的RAW 264.7巨噬细胞NO产生具有浓度依赖性的抑制作用。这种基于APG与BCNs复合物协同稳定的Pickering乳液界面组装构建的复合水凝胶,有效解决了海藻酸盐对疏水药物负载率低的关键技术瓶颈,展现出pH响应可控释放、生物相容性良好及抗菌抗炎活性显著等综合优势,在感染性创面敷料领域展现出巨大的应用潜力。

     

    Abstract: To address the inherent limitation of alginate-based hydrogels in loading hydrophobic drugs, this study developed a composite hydrogel (Alg-APG/BCNs) by encapsulating drug-loaded Pickering emulsions within an alginate hydrogel matrix. This was achieved through a synergistic strategy combining the drug-loading performance of Pickering emulsions co-stabilized by dodecyl glycoside (APG) and bacterial cellulose nanocrystals (BCNs) with calcium ion-induced internal crosslinking, enabling effective loading and controlled release of the hydrophobic antimicrobial agent triclosan (TCA). BCNs with a zeta potential of -33.4 mV and an average particle size of 454.1 nm were prepared via sulfuric acid hydrolysis and hydrogen peroxide oxidation of bacterial cellulose. Drug-loaded Pickering emulsions were then formulated using APG/BCNs composites as an efficient emulsifying system, with TCA-dissolved chloroform as the oil phase under high-speed shearing. Subsequently, the drug-loaded Pickering emulsions were uniformly mixed with alginate solution, and internal crosslinking was triggered by the CaCO3/D-(+)-glucono-δ-lactone (GDL) system, resulting in the formation of a structurally stable composite hydrogel with the emulsions uniformly encapsulated within the alginate three-dimensional network. Experimental results demonstrated that the fabricated Alg-APG/BCNs composite hydrogel possessed a high porosity of 91.60% ± 3.7%, achieved an encapsulation efficiency of 91.5% ± 3.8% for TCA, and exhibited a sustained release profile over 160 h with pH-responsive characteristics. Moreover, the composite hydrogel showed favorable cytocompatibility toward L929 cells within the concentration range of 50–400 μg/mL, displayed significant antibacterial activity against both Gram-negative Escherichia coli and Gram-positive Staphylococcus aureus, and exerted a concentration-dependent inhibitory effect on nitric oxide (NO) production in lipopolysaccharide (LPS)-induced RAW 264.7 macrophages. Collectively, the Alg-APG/BCNs composite hydrogel, constructed via interfacial assembly of APG/BCNs co-stabilized Pickering emulsions, effectively overcomes the key technical bottleneck of low hydrophobic drug loading capacity in alginate-based systems, offering combined advantages of pH-responsive controlled release, favorable biocompatibility, and potent antibacterial and anti-inflammatory activities, thereby holding great promise for application in infected wound dressings.

     

/

返回文章
返回