气膜孔几何特征对氧化铝陶瓷基复合材料拉伸损伤演化与强度的影响

Effect of film cooling hole geometry on tensile damage evolution and strength of Al2O3/Al2O3 composites

  • 摘要: 针对含气膜孔Al2O3/Al2O3复合材料在拉伸载荷下的响应与损伤演化问题,发展了一种基于渐进损伤理论的数值分析方法。该方法以最大应变失效准则与ZWT非线性本构方程为基础,通过参数化建模建立含气膜孔结构的有限元模型,实现了Al2O3/Al2O3材料在拉伸载荷下的响应和损伤演化规律的分析。与试验结果对比表明,模型预测强度与实测值吻合良好(最大误差约4.86%),验证了该方法在预测材料强度及损伤扩展行为方面的有效性。进一步建立了以气膜孔倾角、孔径及孔型等几何参数为变量的参数化有限元模型,揭示了各参数对拉伸响应及损伤演化规律的影响。结果表明:气膜孔倾角对拉伸强度的影响相对有限;孔径增大导致应力集中增强,拉伸强度显著降低;对于扇形孔结构,大孔径侧率先萌生损伤并向小孔径侧扩展,孔径差的增大加速了失效进程,表明控制孔径差比单纯限制单侧孔径更能有效延缓失效。

     

    Abstract: To address the tensile response and damage evolution of Al2O3/Al2O3 composites containing film cooling holes, a numerical analysis method based on progressive damage theory was developed. This method integrated the maximum strain failure criterion with the ZWT nonlinear constitutive equation. Through parametric modeling, a finite element model was established to analyze the tensile response and damage evolution of the composites. Agreement between the predicted and measured strengths (maximum error of approximately 4.86%) validates the effectiveness of the method in predicting strength and damage propagation. Furthermore, the influences of geometric parameters—including hole inclination angle, diameter, and hole shape—on the tensile response and damage evolution were systematically investigated. The results indicate that the hole inclination angle has a relatively limited effect on tensile strength. Increasing the hole diameter enhances stress concentration, leading to a significant reduction in tensile strength. For the fan-shaped hole structure, damage initiates first on the larger-diameter side and propagates toward the smaller-diameter side. A larger diameter difference accelerates the failure process, indicating that controlling the diameter difference is more effective in delaying failure than simply limiting the diameter on a single side.

     

/

返回文章
返回