Abstract:
To clarify the effects of carbon nanotubes (CNTs) on pore–crack structures, interfacial stress and damage paths, concrete containing 50% recycled coarse aggregate and 50% iron tailings sand was investigated at CNT dosages of 0–0.15% by cement mass. Compression tests, scanning electron microscopy (SEM), mercury intrusion porosimetry (MIP), industrial computed tomography (CT) and acoustic emission (AE) measurements were performed, and a CNT–mortar equivalent cell and three- and two-dimensional mesoscopic models were established. The mean 28 d compressive strength first increased and then decreased with increasing CNT dosage. At 0.10% CNT, it increased from 51.13 to 60.56 MPa, an increase of approximately 18.45%, while the corresponding porosity measured by MIP decreased from 17.66% to 14.33%. CT reconstructions after unloading showed a more dispersed distribution of resolvable cracks in the modified concrete. The equivalent cell yielded a mortar elastic-modulus increment of approximately 3 500 MPa, and the peak stresses predicted by both mesoscopic models agreed with the experimental results, with absolute errors below 5%. The stress-concentration coefficient of the old–new interface decreased from 1.63 to 1.27, a reduction of approximately 22.1%. Within the investigated material and loading ranges, an appropriate CNT dosage improved matrix continuity and adjusted multiphase stress transfer, thereby dispersing damage and increasing compressive load capacity.