冻融循环后重组竹力学性能劣化研究

Deterioration of Mechanical Properties of Bamboo Scrimber Subjected to Freeze-Thaw Cycles

  • 摘要: 为研究冻融循环作用下重组竹力学性能的退化规律及其损伤机制,本文对0、100、200和300次冻融循环下重组竹试件开展抗拉、抗压和抗弯试验研究,并结合扫描电子显微镜(SEM)测试、能谱分析(EDS)、傅里叶变换红外光谱仪(FTIR)测试、X 射线衍射(XRD)测试对其微观形貌、化学组成、特征官能团及相对结晶度指标变化进行分析。结果表明:随着冻融循环次数由0次增加至300次,重组竹抗拉、抗压和抗弯强度分别下降16.11%、28.68%和20.29%,对应弹性模量分别下降18.81%、22.31%和17.05%,抗压性能退化最为明显。0~300次冻融范围内,各力学性能指标可用线性关系近似描述。微观结果显示,相对结晶度指标由2.79%降至1.30%,裂纹面积率和界面脱黏率分别由约0.6%和0.3%增至8.7%和7.6%,表明性能衰减与微观损伤累积、界面劣化及晶区有序程度下降密切相关。基于试验结果,建立了考虑冻融循环次数的重组竹力学性能计算公式,可为重组竹材料在滨海、严寒等地区的应用提供依据。

     

    Abstract: To investigate the degradation behavior and damage mechanism of bamboo scrimber under freeze–thaw cycles, this study subjected reconstituted bamboo specimens to 0, 100, 200, and 300 freeze–thaw cycles, and carried out tensile, compressive, and flexural tests. Combined with scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), Fourier transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD) tests were conducted to analyze the changes in micro-morphology, chemical composition, characteristic functional groups, and relative crystallinity indicator. The results showed that, as the number of freeze–thaw cycles increased from 0 to 300, the tensile, compressive, and flexural strengths of bamboo scrimber decreased by 16.11%, 28.68%, and 20.29%, respectively, while the corresponding elastic moduli decreased by 18.81%, 22.31%, and 17.05%, respectively, with the degradation of compressive properties being the most pronounced. Within the range of 0–300 freeze–thaw cycles, the mechanical property indicators could be approximately described by linear relationships. The microscopic results showed that the relative crystallinity index decreased from 2.79% to 1.30%, while the crack area ratio and interfacial debonding ratio increased from approximately 0.6% and 0.3% to 8.7% and 7.6%, respectively. These results indicate that the deterioration of mechanical properties was closely associated with accumulated microstructural damage, interfacial degradation, and reduced ordering of crystalline regions. These results indicate that the deterioration of mechanical properties is associated with accumulated microstructural damage, interfacial degradation, and reduced ordering of crystalline regions. Based on the experimental results, a calculation formula for the mechanical properties of reconstituted bamboo considering the number of freeze–thaw cycles was established, which can provide a basis for its application in coastal and cold regions.

     

/

返回文章
返回