盐冻作用下UHPC-NC组合梁层厚效应与承载力模型

Thickness effect and bearing capacity model of UHPC-NC composite beams subjected to salt freeze-thaw cycles

  • 摘要: 为系统揭示盐冻环境下超高性能混凝土(UHPC)层厚度对UHPC-普通混凝土(NC)组合梁受弯性能的影响规律,建立了考虑盐冻损伤的承载力退化模型,本文基于试验研究与理论分析方法,对配置6种不同UHPC层厚度的12根组合梁开展了90次盐冻循环加速试验及四点弯曲试验,并结合微观分析,探讨了UHPC层厚度对组合梁宏观力学响应和微观损伤演化的作用机制。结果表明,UHPC层凭借其致密的微观结构有效阻滞了氯离子侵蚀与冻融损伤,当厚度达到梁高的1/6时,可为结构提供充分的耐久性保障。在力学性能方面,UHPC层的引入显著提升了组合梁的开裂荷载,与0 mm UHPC的NC基准梁相比,25 mm UHPC层试件的开裂荷载和极限承载力分别提高105%和47%。所建立的耦合材料性能退化与截面损伤的承载力模型,其预测值与试验值吻合良好,最大误差为9.7%,可为严酷环境下此类复合结构的设计提供理论支撑。

     

    Abstract: To systematically reveal the influence of the ultra-high performance concrete (UHPC) layer thickness on the flexural performance of UHPC–normal concrete (NC) composite beams under salt freeze-thaw conditions, and to develop a load-bearing capacity degradation model that accounts for salt freeze–thaw damage, this study presents an experimental and theoretical investigation. A total of 12 composite beams with six different UHPC layer thicknesses were subjected to 90 salt freeze-thaw cycles, followed by four-point bending tests. The mechanisms through which the UHPC layer thickness affects the macro-mechanical response and micro-damage evolution were explored via microstructural analysis. The results indicate that the dense microstructure of the UHPC layer effectively impedes chloride ingress and freeze-thaw damage. A thickness equivalent to 1/6 of the beam height was found to provide sufficient durability protection. Mechanically, relative to the NC control beams without a UHPC layer, the specimens with a 25 mm UHPC layer showed increases of 105% in cracking load and 47% in ultimate load capacity. A bearing capacity model coupling material degradation and section damage was established, and its predictions showed good agreement with experimental results, with a maximum error of 9.7%. This work provides a theoretical basis for the design of such composite structures in harsh environments.

     

/

返回文章
返回