Synergistically toughening epoxy resins with reactive acrylate-based block copolymers and nano-SiO2

  • 摘要: 利用引发剂可连续再生催化剂原子转移自由基聚合(ICAR-ATRP)合成了两种反应性丙烯酸酯三嵌段共聚物:聚(甲基丙烯酸甲酯-co-甲基丙烯酸缩水甘油酯)-b-聚丙烯酸丁酯-b-聚(甲基丙烯酸甲酯-co-甲基丙烯酸缩水甘油酯) (PMGBMG)和聚甲基丙烯酸甲酯-b-聚(丙烯酸丁酯-co-甲基丙烯酸缩水甘油酯)-b-聚甲基丙烯酸甲酯(PMBGM)。并将硅烷偶联剂KH-550改性的纳米SiO2接枝于嵌段共聚物,用于对环氧树脂E-51进行增韧。研究结果表明:仅加入5%PMGBMG-SiO2,相对纯E-51体系其断裂韧性参数临界应力强度因子(KIC)提高了145%,拉伸强度和模量分别提高了8%和31%,明显优于不接枝的嵌段共聚物和PMBGM-SiO2,实现了韧性和刚性的同时提高,并且材料的耐热性保持较好。

     

    Abstract: Two reactive acrylate triblock copolymers including poly(methyl methacrylate-co-glycidyl methacrylate)-b-poly(butyl acrylate)-b-poly(methyl methacrylate-co-glycidyl methacrylate) (PMGBMG) and poly(methyl methacrylate)-b-poly(butyl acrylate-co-glycidyl methacrylate)-b-poly(methyl methacrylate) (PMBGM) were synthesized via initiator for continuous activator regeneration atom transfer radical polymerization (ICAR-ATRP). Nano-SiO2 modified by 3-ainopropyltriethoxysilane (KH-550) was grafted on block copolymer to prepare PMGBMG-SiO2 and PMBGM-SiO2 as tougheners for epoxy resin. Results show that addition of 5%PMGBMG-SiO2 in E-51 epoxy resin can increase the critical stress intensity factor (KIC) by 145% compared with pure epoxy matrix. Meanwhile, the tensile strength and modulus are increased by 8% and 31% respectively, which are superior to the resins modified by pure copolymer and PMBGM-SiO2. The toughness and rigidity are improved simultaneously, while heat resistance is also well maintained.

     

/

返回文章
返回